Compare with traditional PVC base layer, LORIKA®film
creatively adopted ASA alloy material which has high weathering resistance,
consequently, completely solved the color fading problem.
Moreover, The tensile strength and thermal endurance of ASA
base layer is much higher than plasticized PVC layer, then avoid foil
deformation problem during the lamination process and ensured the adhesive
force. |
|
|
|
|
|
LORIKA®film laminating
stretch test:
Film
original width: 52.5 mm
Film
width after laminated on the profile: 52.16 mm
Total
stretch: 0.34 mm
|
Domestic PVC/PMMA film laminating stretch test:
Film
original width: 51.7 mm
Film
width after laminated on the profile:
the widest:46.9mm the narrowest:45.8mm
Total
stretch: 4.8 mm-5.9 mm
|
|
|
LORIKA®film adhesion test |